A Preliminary Evaluation into the Performance of Posterior Resin Bonded Cast Metal Restorations (Adhesive Onlays)
doi:10.1922/EJPRD_1067Marchan05
Abstract - Posterior resin bonded cast metal restorations (adhesive onlays) were used in a variety of clinical scenarios including: management of tooth wear and cracked tooth, as retainers for fixed bridge work, for correction of the occlusal plane and in providing cuspal coverage following endodontic treatment. The mean length in service for the examined onlays was 42 months, with a range of 9-75 months. Two restorations in two patients failed resulting in an overall success of 94%. Patient satisfaction was high at 95%. Such restorations seem to be a viable option for managing a number of clinical scenarios.
KEY WORDS: Resin bonded cast metal restorations, adhesive onlays, cracked tooth, bridge retainers, tooth wear
- Article Price
- £15.00
- Institution Article Price
- £
- Page Start
- 24
- Page End
- 28
- Authors
- S.M. Marchan, A. Eder, Q.M. Marchan, L. Coldero, A.Tang Choon, W.A. Smith
Articles from this issue
- Title
- Pg. Start
- Pg. End
- A Simple Method to Fabricate Stabilized Record Bases: A Modified Approach Using Casting Wax for the Borders
- 2
- 4
- Effect of Artificial Saliva and pH on Shear Bond Strength of Resin Cements to Zirconia-Based Ceramic
- 5
- 8
- Unilateral Bounded Saddles: A Clinical Case Report on the use of a Two Part Sectional Removable Partial Denture
- 16
- 23
- A Preliminary Evaluation into the Performance of Posterior Resin Bonded Cast Metal Restorations (Adhesive Onlays)
- 24
- 28
- A Study to Evaluate the Prevalence of Golden Proportion and RED Proportion in Aesthetically Pleasing Smiles
- 29
- 33
- Provision of an Appliance to Correct Mandibular Deviation Secondary to Temporomandibular Joint Replacement
- 40
- 43
- Evaluation and Comparison of the Internal Fit and Marginal Accuracy of Base Metal (Nickelchromium) and Zirconia Copings Before and after Ceramic Veneering: A Sem Study
- 44
- 48