Fracture of Zirconia Abutment with Metallic Insertion on Anterior Single Titanium Implant with Internal Hexagon: Retrieval Analysis of a Failure
ABSTRACT
This case report presents a retrieval analysis of a screw-retained one-piece restoration with the veneering ceramic fired directly onto the zirconia abutment that fractured during insertion. A patient who experienced root fracture of a maxillary left central incisor received a titanium implant on the same day as extraction. After delayed implant loading, a two-piece zirconia abutment with metallic insertion was customized. Upon installation, a horizontal fracture of the crown just above the metallic portion was detected. The retrieval analysis of a fractured zirconia abutment showed crack formation and diffusion of glaze material that expanded the crack line during firing.
Keywords
Dental Implants
Zirconia
Prosthesis Failure Analyses
Periprosthetic Fractures
Dental Implant-Abutment Design
Dental Porcelain
doi: 10.1922/EJPRD_01556Bottino05
- Article Price
- £15.00
- Institution Article Price
- £
- Page Start
- 164
- Page End
- 168
- Authors
- Prof. Marco Antonio Bottino, Dr Regina Furbino Villefort Rocha, Dr Lilian Costa Anami, Dr Mutlu Özcan, Dr Renata Marques de Melo
Articles from this issue
- Title
- Pg. Start
- Pg. End
- ‘Own-Label’ Versus Branded Commercial Dental Resin Composite Materials: Mechanical And Physical Property Comparisons
- 122
- 129
- Marginal Adaptation, Gap Width, and Fracture Strength of Teeth Restored With Different All-Ceramic Vs Metal Ceramic Crown Systems: An in Vitro Study
- 130
- 137
- Anti-Inflammatory and Regenerative Effects of Albanian Propolis in Experimental Vital Amputations
- 145
- 151
- Fracture of Zirconia Abutment with Metallic Insertion on Anterior Single Titanium Implant with Internal Hexagon: Retrieval Analysis of a Failure
- 164
- 168